| Application Instructions |
| |
| Step One: |
PREP |
|
Make sure surface is clean, dry & in good condition. Clean weathered wood with Messmer’s WD Wood &
Deck Renewer. Remove previous stain or paint completely before applying UV
Plus. Apply when temperatures are between 40-95ºF, and surface is
not hot to the touch. Do not thin. |
| |
| Step Two: |
MIX |
|
Stir well initially and continue to mix during use. Intermix all containers of the same color to
ensure uniform appearance. Cover plants, grass and concrete to protect from spills. Contains natural oils |
| |
| Step Three: |
TEST |
|
Apply to a small test area to ensure complete penetration and color satisfaction before
proceeding with the entire project. |
| |
| Step Four: |
EQUIP |
|
Apply with a quality bristle brush, roller, pad, or airless sprayer. Brush or back roll if applied by spray. |
| |
| Step Five: |
APPLY |
|
Apply a uniform, even coat. Stain the full length of boards, keeping a wet
edge. One coat is sufficient for most applications. On decks, excess product not absorbed within 30-45 minutes
must be removed to prevent tackiness and surface sheen. |
| |
| Step Six: |
CLEAN |
|
Clean application equipment with mineral spirits (paint thinner). |
| |
| |